Find's Treasure Forums

Welcome to Find's Treasure Forums, Guests!

You are viewing this forums as a guest which limits you to read only status.

Only registered members may post stories, questions, classifieds, reply to other posts, contact other members using built in messaging and use many other features found on these forums.

Why not register and join us today? It's free! (We don't share your email addresses with anyone.) We keep email addresses of our users to protect them and others from bad people posting things they shouldn't.

Click here to register!



Need Support Help?

Cannot log in?, click here to have new password emailed to you

Changed email? Forgot to update your account with new email address? Need assistance with something else?, click here to go to Find's Support Form and fill out the form.

Got A First...A Partially Started Coin Ring And A Silver Ring. What Are The Chances:shrug:

John-Edmonton

Moderator
Staff member
I headed out after work for a couple of hours. My third signal turned out to be a US Quarter, with the outside edges partially hammered, a way to make a coin ring with a shiny outside. Also found a silver ring..... my last find of the evening. I headed home and finished the coin-ring.

Below is a link to an article "COIN RING CRAFTING" I wrote for Western And Eastern Treasure many years ago:

http://www.detectorplace.com/detecting/Coinrings/HowtomakeaCoinRings.pdf
 
Fascinating read, John. Thanks for sharing...and writing. I had forgotten you did these. Impressive talent!
 
Thanks for the PDF John. Any video tutorials next ???
 
Here's a Video On Coin-ring Making https://www.youtube.com/watch?v=Ojv19Eh5tTM


Here's one on making shotgun shell rings. https://www.youtube.com/watch?v=Ak1efE17Ito
 
Thanks John. Very nice. I'm just wondering about the purpose of the annealing process over heat. Is it only to change the appearance ?
 
The annealing process softens the metal. After a coin, shotgun shell is pressed from a die, it is very hard. If you try to stretch/bend copper/silver/brass, it will crack or split. So, you anneal before doing any serious bending or stretching, which brings it back to a soft state. Don't let it get too red, or it can blister. A nice dull pink works well. You can either quench it in water, a pickling solution or let it air cool. Using a pickling solution keeps the surface from oxidizing while it is cooling down.

Below is a recipe for home made pickling solution.

http://www.natashalh.com/tutorial-thursday-recipe-to-make-your-own-natural-jewelers-pickle/
 
That walking liberty ring ! Awesome. I was thinking of turning the 1967 silver cougar/bobcat quarter into a ring. I think it would look really nice with the animal right in the middle of the ring.
 